+ | I believe there are two problems: | ||
+ | |||
+ | * There are veins of impurities running through the glass. | ||
+ | ** These will create a week point for a crack to start. | ||
+ | * My tempering profile could be improved. | ||
+ | ** The current profile I'm using was created for tempering float glass. Container glass is slightly different, and so may require a different profile. | ||